High hardness and wear resistance, both impingement and frictional modes
Superior thermal shock resistance
Low thermal expansion
Electrical insulator
Good oxidation resistance
Good chemical corrosion resistance
Wear resistant
High stiffness
Sign In | Join Free | My portofva.com |
|
Brand Name : BLM
Model Number : BLM-S
Certification : ISO
Place of Origin : Jiangsu,China
MOQ : 100kgs
Price : Negtation
Payment Terms : T/T
Supply Ability : 5 tons per month
Delivery Time : 25days
Packaging Details : Packing with wooden box
Name : Si3N4 Silicon Nitride Ceramic Dowel Pin
Application : Industrial ceramic
Material : Silicon nitride ceramic
Product name : Ceramic dowel pin
Color : Dark grey to black
Feature : High hardness
Advantage : Insulation etc.
Thermal shock resistance : 750
Dielectric loss : 3.8*10-4HMZ
Elastic Modulus : 320
Place of origin : Jiangsu,China
Ceramic Nitride Silicone Si3N4 Pin For Welding Nut
1 . Description:
Silicon nitride ceramics have good tribological properties and excellent fracture toughness, which makes it be predestined for applications as balls and rolling elements for light and extremely precise bearings, heavy-duty ceramic forming tools and automotive components subject to high stress. And the good thermal shock resistance and high temperature resistance is exploited in welding processes.
2 . Advantages of silicon nitride ceramic dowel pin
High hardness and wear resistance, both impingement and frictional modes
Superior thermal shock resistance
Low thermal expansion
Electrical insulator
Good oxidation resistance
Good chemical corrosion resistance
Wear resistant
High stiffness
3 . Applications of silicon nitride ceramic
✔ Welding pins, jigs, fixtures and nozzles
✔ Turbine blades
✔ Bearing balls and rollers
✔ Cutting tools
✔ Valves, turbocharger rotors for engines
✔ Diesel engine glow plugs
✔ Molten metal handling
✔ Thermocouple sheaths
Properties of silicon nitride ceramic
Properties | Condition | Units | Silicon Nitride(Si3N4) |
Density | | g/cm^3 | 3.21 |
Flexural Strength (MOR) | 20 ℃ | Mpa | 800 |
Elastic(Young's) Modulus | 20℃ | GPa (psi x 10^6) | 320 |
Compressive Strength | 20℃ | MPa (psi x 10^3) | 3000 |
Hardness(Vickers) | | GPa | 16 |
Fracture Toughness | K(I c) | Mpa m^1/2 | 6.5 |
Thermal Conductivity | 20℃ | W/m °K | 28 |
Coefficient of Thermal Expansion | 25-1000 ℃ | 1X 10^-6 /℃ | 3.5 |
Specific Heat | 100 ℃ | J/kg*K | 740 |
Dielectric Strength | 6.35mm | ac-kV/mm (ac V/mil) | 8.6 |
Dielectric Constant | 25 ℃ | 1 MHz | 8.15 |
Volume Resistivity | 25 ℃ | ohm-cm | 10^14 |
![]() |
Si3N4 Silicon Nitride Ceramic Dowel Pin For Welding Nut Images |